MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Architectural Bronze, UNS C38500
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass; Bronze

Material Notes: This is technically a brass alloy (copper plus zinc) but is known as architectural bronze. Fair to excellent corrosion resistance. Excellent machinability and hot workability. Fabricated by hot forging and pressing, forming, bending and machining.

Applications: architectural extrusion, store fronts, thresholds, trim, butts, hinges, lock bodies and forgings.

Available as rod, shapes.

Key Words: British Free Machining Brass, BS 2874 CZ121, ISO CuZn39Pb3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6565M30 temper
Tensile Strength, Ultimate 415 MPa60200 psiM30 temper
Tensile Strength, Yield 140 MPa
@Strain 0.5 %
20300 psi
@Strain 0.5 %
M30 temper
Elongation at Break 30 %30 %in 50 mm, M30 temper
Modulus of Elasticity 97.0 GPa14100 ksi
Poissons Ratio 0.310.31Calculated
Machinability 90 %90 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 37.0 GPa5370 ksi
Shear Strength 240 MPa34800 psiM30 temper
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
0.00000620 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.9 µm/m-°C
@Temperature 20.0 - 300 °C
11.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 123 W/m-K
@Temperature 20.0 °C
854 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 875 - 890 °C1610 - 1630 °F
Solidus 875 °C1610 °F
Liquidus 890 °C1630 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 625 - 725 °C1160 - 1340 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 55 - 60 %55 - 60 %
Iron, Fe <= 0.35 %<= 0.35 %
Lead, Pb 2.0 - 3.8 %2.0 - 3.8 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 40 %40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Architectural Bronze, UNS C38000
Forging Brass, UNS C37700
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy
Mueller Alloy 3850 Architectural Brass (UNS C38500)

MC38500b1 / 11254

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.