MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chicago Extruded Metals UNS C37700 Copper-Zinc-Lead Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Copper-Zinc-Lead Alloy (Leaded Brass)

Finished product available as bar, rod, forged, or shapes.
Chicago Extruded Metal temper codes: H01, H02, M30

Information provided by Chicago Extruded Metals

Key Words: CDA 377, ASM 4614, ASTM B124
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.44 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 359 MPa52000 psi
Tensile Strength, Yield 138 MPa20000 psi
Elongation at Break 45 %45 %
Machinability 80 %80 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000639 ohm-cm0.00000639 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 119 W/m-K828 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 58 - 61 %58 - 61 %
Iron, Fe 0.30 %0.30 %
Lead, Pb 1.5 - 2.5 %1.5 - 2.5 %
Other, total 0.50 %0.50 %
Zinc, Zn 35.7 - 39.7 %35.7 - 39.7 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Forging Brass, UNS C37700
Mueller Alloy 3770 Forging Brass (UNS C37700)
Architectural Bronze, UNS C38000
Chicago Extruded Metals UNS C38000 Copper-Zinc-Lead Alloy
Aluminum 2014-O

NCHICA913 / 147632

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.