MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast/AboCure 8109-6
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: High heat resistance. Easy to use.

Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.

Applications: Castings and laminates for high temperature applications.

Key Words: castings, laminating, laminates
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
Water Absorption 0.15 - 0.20 %0.15 - 0.20 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
 0.20 - 0.30 %0.20 - 0.30 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
Viscosity 1000 - 2500 cP1000 - 2500 cP
Vapor Pressure  <= 0.0000267 bar
@Temperature 50.0 °C
<= 0.0200 torr
@Temperature 122 °F
AboCure
 <= 0.00133 bar
@Temperature 180 °C
<= 1.00 torr
@Temperature 356 °F
AboCast
 0.00200 bar
@Temperature 100 °C
1.50 torr
@Temperature 212 °F
AboCure
 0.0293 bar
@Temperature 165 °C
22.0 torr
@Temperature 329 °F
AboCure
 0.0667 bar
@Temperature 180 °C
50.0 torr
@Temperature 356 °F
AboCure
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.84 MPa11000 psi
Modulus of Elasticity 3.102 GPa449.9 ksi
Flexural Yield Strength 131 MPa19000 psi
Compressive Yield Strength 137.9 MPa20000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.50e+16 ohm-cm>= 1.50e+16 ohm-cm
Dielectric Constant  3.3 - 3.5
@Frequency 1e+6 Hz
3.3 - 3.5
@Frequency 1e+6 Hz
 3.4 - 3.6
@Frequency 1000 Hz
3.4 - 3.6
@Frequency 1000 Hz
 3.6 - 3.8
@Frequency 50 Hz
3.6 - 3.8
@Frequency 50 Hz
Dielectric Strength 13.8 - 17.7 kV/mm
@Thickness 3.17 mm
350 - 450 kV/in
@Thickness 0.125 in
Short time value
Dissipation Factor  0.0020 - 0.0040
@Frequency 50 Hz
0.0020 - 0.0040
@Frequency 50 Hz
 0.0030 - 0.0050
@Frequency 1000 Hz
0.0030 - 0.0050
@Frequency 1000 Hz
 0.010 - 0.015
@Frequency 1e+6 Hz
0.010 - 0.015
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 - 65.0 µm/m-°C
@Temperature 20.0 °C
30.6 - 36.1 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 150 °C302 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °F
Pot Life  420 - 600 min
@Temperature 120 °C
420 - 600 min
@Temperature 248 °F
 21600 - 28800 min
@Temperature 20.0 °C
21600 - 28800 min
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE 4430 KIT
Dow SE 4420 THERMALLY CONDUCTIVE ADHESIVE
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Overview of materials for Epoxy Adhesive
NRI Thermo-Wrap™

PABEU1 / 22020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.