MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NRI Thermo-Wrap™
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Description: Thermo-Wrap™ is a custom engineered composite system utilizing a high strength, bidirectional, woven fiberglass tape in conjunction with NRI’s proprietary Thermo-Poxy™ epoxy system for the repair and restoration of pipes operating at elevated temperatures. This operator qualified engineered system was designed to conform to and recognized by ASME PCC-2, ASME B31, ISO TS24817, DOT, API, and CSA Z662 standards for nonmetallic reinforcing solutions, thus ensuring product application integrity. Thermo-Wrap is specifically designed for repair applications which require the composite to maintain the high design strengths in high temperature environments, while still curing under room temperature conditions.

Typical Applications:

  • Flare lines
  • Steam piping
  • Girth welds, elbows, tees
  • Chemical processing lines
  • Anywhere elevated temperatures are of concern or expected
Benefits:
  • High temperature rating with an ambient cured epoxy
  • No heating or post-curing required
  • Full factory engineering calculations, consultation, and support ensuring safe and successful repairs

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D2240
Tensile Strength  487 MPa
@Temperature 149 °C
70600 psi
@Temperature 300 °F
ASTM D3039
 700 MPa
@Temperature 23.0 °C
102000 psi
@Temperature 73.4 °F
ASTM D3039
Tensile Modulus  24.6 GPa
@Temperature 149 °C
3570 ksi
@Temperature 300 °F
ASTM D3039
 30.9 GPa
@Temperature 23.0 °C
4480 ksi
@Temperature 73.4 °F
ASTM D3039
Flexural Strength 839.1 MPa121700 psiASTM D790
Flexural Modulus 28.8 GPa4180 ksiASTM D790
Shear Modulus 4.34 GPa629 ksiChord; ASTM D5379
Shear Strength 25.5 MPa3700 psiLap (to steel); ASTM D5868
 90.011 MPa13055 psiIn-Plane; ASTM D5379
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.79 µm/m-°C3.77 µin/in-°FASTM E831
Maximum Service Temperature, Air 149 °C300 °F
Heat Distortion Temperature 268 °C514 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 5.00 - 93.0 °C41.0 - 199 °FApplication Range
Cure Time 1080 min
@Temperature 24.0 °C
18.0 hour
@Temperature 75.2 °F
Pot Life 75.0 min75.0 min
Working Life 45.0 min
@Temperature 24.0 °C
45.0 min
@Temperature 75.2 °F
Gel Time 161 min
@Temperature 21.0 °C
161 min
@Temperature 69.8 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
Overview of materials for Epoxy/Carbon Fiber Composite
Hybrid Plastics FireQuench® PM 1287 Resin
Epoxy Technology EPO-TEK® H70E Thermally Conductive, Electrically Insulating Epoxy
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)

PNRI024 / 192040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.