MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Carpenter 20-Mo6® Stainless Steel, Plate
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, crevice corrosion and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. The alloy is designed for applications where better pitting and crevice-corrosion resistance are requires than 20Cb-3® stainless offers.

20-Mo6® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS N08026
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.133 g/cc0.2938 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8585
Tensile Strength, Ultimate 641 MPa93000 psi
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
45000 psi
@Strain 0.2 %
Elongation at Break 50 %50 %
Reduction of Area 80 %80 %
Modulus of Elasticity 186 GPa27000 ksi
Poissons Ratio 0.290.29
Shear Modulus 72.1 GPa10500 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0001082 ohm-cm0.0001082 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.8 µm/m-°C
@Temperature 25.0 - 100 °C
8.22 µin/in-°F
@Temperature 77.0 - 212 °F
 15.34 µm/m-°C
@Temperature 25.0 - 300 °C
8.522 µin/in-°F
@Temperature 77.0 - 572 °F
 16.01 µm/m-°C
@Temperature 25.0 - 500 °C
8.894 µin/in-°F
@Temperature 77.0 - 932 °F
 17.74 µm/m-°C
@Temperature 25.0 - 900 °C
9.856 µin/in-°F
@Temperature 77.0 - 1650 °F
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°F
Thermal Conductivity  12.1 W/m-K
@Temperature 50.0 °C
84.0 BTU-in/hr-ft²-°F
@Temperature 122 °F
 14.8 W/m-K
@Temperature 200 °C
103 BTU-in/hr-ft²-°F
@Temperature 392 °F
 18.2 W/m-K
@Temperature 400 °C
126 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 22 - 26 %22 - 26 %
Copper, Cu 2.0 - 4.0 %2.0 - 4.0 %
Iron, Fe 31 %31 %as remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 5.0 - 6.7 %5.0 - 6.7 %
Nickel, Ni 33 - 37 %33 - 37 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson C 825 Nickel-Iron-Chromium Alloy
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age
Carlson 20 Plus Alloy
Carlson 904L Austenitic Stainless Steel

NCARJ0 / 15786

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.