MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Carlson 904L Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: General Description

904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a wide range of both oxidizing and reducing environments. The high nickel content also provides resistance to chloride stress corrosion cracking.

Molybdenum and copper are present in the alloy for increased resistance to pitting and crevice corrosion and to general corrosion in reducing acids.

The low carbon content of 904L provides resistance to intergranular corrosion in the post-welded or stress relieved condition.

Applications

The corrosion resistance of 904L makes it a useful alloy in numerous severe operating environments. It is utilized extensively in the chemical, petrochemical, pulp and paper, and pollution control industries :

  • Tanks, vessels, piping, heat exchangers, and other equipment for the production and handling of sulfuric and phosphoric acid.
  • Reactor vessels for fertilizer production
  • Tall oil distillation
  • Pulp and paper bleaching operations
  • Absorber towers, stack linings, duct work, dampers, and other support equipment for flue gas desulphurization systems for fossil-fired power plants and waste incinerators.

Information provided by Carlson

Key Words: UNS N08904
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.97 g/cc0.288 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 192<= 192
Hardness, Rockwell B <= 90<= 90
Tensile Strength at Break >= 490 MPa>= 71000 psi
Tensile Strength, Yield >= 214 MPa
@Strain 0.2 %
>= 31000 psi
@Strain 0.2 %
Elongation at Break >= 35 %>= 35 %
Reduction of Area >= 40 %>= 40 %
Modulus of Elasticity 196 GPa28400 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 20.0 - 98.9 °C
5.80 µin/in-°F
@Temperature 68.0 - 210 °F
 14.6 µm/m-°C
@Temperature 20.0 - 399 °C
8.10 µin/in-°F
@Temperature 68.0 - 750 °F
 16.6 µm/m-°C
@Temperature 20.0 - 799 °C
9.20 µin/in-°F
@Temperature 68.0 - 1470 °F
Specific Heat Capacity 0.439 J/g-°C
@Temperature 20.0 °C
0.105 BTU/lb-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 19 - 23 %19 - 23 %
Copper, Cu 1.0 - 2.0 %1.0 - 2.0 %
Iron, Fe 38.9 - 53 %38.9 - 53 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 4.0 - 5.0 %4.0 - 5.0 %
Nickel, Ni 23 - 28 %23 - 28 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.035 %<= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 904L High Performance Austenitic Stainless Steel
317LN High-Nitrogen Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S31753
Type 904L Austenitic Stainless Steels, Annealed Bar, UNS N08904
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
AK Steel 316 Austenitic Stainless steel

NCARLSO04 / 15811

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.