MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Astralloy Astralloy-V® Air Hardened Wear Steel Plate
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: Astralloy-V® is a deep-air hardened steel. It is through hardened and unsurpassed in resistance to impact and abrasion. With continuous impact and abrasion, Astralloy-V can reach a hardness in excess of 550 BHN without brittleness.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 418 - 512418 - 512
Tensile Strength 1660 MPa241000 psi
Tensile Strength, Yield 1080 MPa157000 psi
Elongation at Break 12 %
@Thickness 50.8 mm
12 %
@Thickness 2.00 in
Charpy Impact 29.8 J22.0 ft-lb
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.29 %<= 0.29 %
Chromium, Cr <= 2.0 %<= 2.0 %
Iron, Fe >= 91.6 %>= 91.6 %As Balance
Manganese, Mn <= 1.2 %<= 1.2 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 4.0 %<= 4.0 %
Phosphorus, P <= 0.0015 %<= 0.0015 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Astralloy 4800® Wear Resistant Steel
ASTM A543 Steel, Grade B
Astralloy BP6:33® Ballistic Resistant Steel Plate
Overview of materials for AISI 4000 Series Steel
Ovako 28NiCrMnMo14-6-4* 455A Steel

NNUCOR900 / 233174

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.