Astralloy-V® is a deep-air hardened steel. It is through hardened and unsurpassed in resistance to impact and abrasion. With continuous impact and abrasion, Astralloy-V can reach a hardness in excess of 550 BHN without brittleness.Information provided by Astralloy, a Nucor Company. |