MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Astralloy BP6:33® Ballistic Resistant Steel Plate
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: With its unique metallurgical characteristics, it can be cut cold and welded using normal shop practices and still retain its high hardness, without loss of ballistic properties. BP6:33 will defeat a wide range of commercial and military threats such as handguns, rifles, automatic weapons, and fragmentation. BP6:33 is independently tested to meet the National Institute of Justice Standards 0108.01 (Level III) and is listed with the Underwriters Laboratories (Standard 752). BP6:33 can be modified to meet testing levels UL 6 & 7, as well as test level NIJ IV at customer’s request on specific gauges.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 477>= 477
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.29 %<= 0.29 %
Chromium, Cr <= 2.0 %<= 2.0 %
Iron, Fe >= 91.6 %>= 91.6 %As Balance
Manganese, Mn <= 1.2 %<= 1.2 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 4.0 %<= 4.0 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Astralloy Astralloy-V® Air Hardened Wear Steel Plate
ERG Aerospace Duocel® Aluminum Metal Foam
HY-100 Steel
Hexcel® HexWeb® CR III 3/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hardwire 12x-23-12 High Density Composite

NNUCOR918 / 233192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.