MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Isoflon Teflon® 20 AD Polytetrafluoroethylene Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Adhesive Skived Pure PTFE Film

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.0 microns1.97 milAdhesive
 500 microns19.7 milBacking
Coating Weight 1080 g/m²675 lb/reamFilm Weight; NF EN ISO 2286.2
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 200 %>= 200 %
Tear Strength 8.80 kN/m50.2 pli
Peel Strength 0.720 kN/m4.11 pli

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Mitsubishi Chemical Advanced Materials Symalit® PVDF (ASTM Product Data Sheet)
Process Technologies Inc Teflon® Sanitary Gasket
Chemours Teflon® PTFE 65 Resin for Lubricated Paste Extrusion
Isoflon Teflon® 10 AD Polytetrafluoroethylene Film

PISOFL936 / 123324

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.