MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Process Technologies Inc Teflon® Sanitary Gasket
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: A very versatile material with broad chemical and temperature resistance and virtually no extractables. PTFE is a plastic and is subject to creep and cold flow. It is not recommended where large temperature variations occur or where component

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.33 °C-99.99 °F
 
Descriptive Properties
Compatibility for ChemicalsAcetoneExcellent
 AmmoniaExcellent
 Hydrochloric AcidExcellent
 Hydrofluoric AcidExcellent
 Hydrogen PeroxideExcellent
 Isopropyl AlcoholExcellent
 Nitric AcidExcellent
 Phosphoric AcidExcellent
 Sodium HydroxideExcellent
 Sodium HypochloriteExcellent
 Steam to 400ºF (204ºC)Limited
 Sulfuric AcidExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Isoflon Teflon® 20 AD Polytetrafluoroethylene Film
Chemours Teflon® FEP CX5010 Fluoropolymer Resin
Chemours Teflon® FEP 121A Aqueous Dispersion
Chemours Teflon® C PFA Grade 510 Static Dissipating Semiconductive Resin

PPTI07 / 138119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.