MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Mitsubishi Chemical Advanced Materials Symalit® PVDF (ASTM Product Data Sheet)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

In January 2016 the Symalit® Fluoroplastics production assets were sold to AGRU Kunststofftechnik GmbH

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Water Absorption 0.030 %0.030 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.050 %0.050 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ASTM D785
Hardness, Shore D 7878ASTM D2240
Tensile Strength 48.3 MPa7000 psiASTM D638
Tensile Strength at 150°C (300°F) 3.45 MPa500 psiASTM D638
Tensile Strength at 65°C (150°F) 27.6 MPa4000 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Tensile Modulus 2.07 GPa300 ksiASTM D638
Flexural Strength 55.2 MPa8000 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Compressive Strength 68.9 MPa10000 psi10% Def.; ASTM D695
Compressive Modulus 1.10 GPa160 ksiASTM D695
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 6.4
@Frequency 1e+6 Hz
6.4
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 10.2 kV/mm260 kV/inShort Term; ASTM D149
Dissipation Factor 0.165
@Frequency 1e+6 Hz
0.165
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 µm/m-°C
@Temperature -40.0 - 149 °C
66.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.216 W/m-K1.50 BTU-in/hr-ft²-°FASTM F433
Melting Point 171 °C340 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 149 °C300 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
Canada AG NoNo
FDA YesYes
NSF YesYes
USDA YesYes
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ColorNatural
Machinability31-10, 1=Easier to Machine

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
Mitsubishi Chemical Advanced Materials Symalit® 1000 PVDF unfilled, extruded (ISO Data)
Arkema Kynar Flex® 2850 WR PVDF
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding

P1SM08A / 20080

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.