MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, Unreinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 - 1.64 g/cc0.0390 - 0.0592 lb/in³Average value: 1.19 g/cc Grade Count:151
 0.932 - 0.932 g/cc
@Temperature >=220 °C
0.0337 - 0.0337 lb/in³
@Temperature >=428 °F
Average value: 0.932 g/cc Grade Count:4
Water Absorption 0.0600 - 9.50 %0.0600 - 9.50 %Average value: 3.89 % Grade Count:67
Moisture Absorption at Equilibrium 0.170 - 3.50 %0.170 - 3.50 %Average value: 2.42 % Grade Count:54
 2.70 - 2.70 %
@Temperature 70.0 - 70.0 °C
2.70 - 2.70 %
@Temperature 158 - 158 °F
Average value: 2.70 % Grade Count:2
Water Absorption at Saturation 8.00 - 10.0 %8.00 - 10.0 %Average value: 9.07 % Grade Count:18
Viscosity 2.60 - 3.00 cP2.60 - 3.00 cPAverage value: 2.63 cP Grade Count:13
Viscosity Test 120 - 145 cm³/g1.20 - 1.45 dl/gAverage value: 130 cm³/g Grade Count:6
Linear Mold Shrinkage 0.00200 - 0.0190 cm/cm0.00200 - 0.0190 in/inAverage value: 0.0115 cm/cm Grade Count:114
Linear Mold Shrinkage, Transverse 0.00400 - 0.0170 cm/cm0.00400 - 0.0170 in/inAverage value: 0.0107 cm/cm Grade Count:59
Melt Flow 8.00 - 260 g/10 min8.00 - 260 g/10 minAverage value: 64.4 g/10 min Grade Count:29
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 97.0 - 12297.0 - 122Average value: 114 Grade Count:37
Hardness, Shore D 71.0 - 83.071.0 - 83.0Average value: 77.0 Grade Count:5
Ball Indentation Hardness 70.0 - 182 MPa10200 - 26400 psiAverage value: 127 MPa Grade Count:6
Tensile Strength, Ultimate 17.0 - 150 MPa2470 - 21800 psiAverage value: 69.0 MPa Grade Count:101
 20.0 - 130 MPa
@Temperature -40.0 - 120 °C
2900 - 18900 psi
@Temperature -40.0 - 248 °F
Average value: 58.3 MPa Grade Count:12
Tensile Strength, Yield 35.0 - 90.3 MPa5080 - 13100 psiAverage value: 64.3 MPa Grade Count:67
 20.0 - 142 MPa
@Temperature -40.0 - 120 °C
2900 - 20600 psi
@Temperature -40.0 - 248 °F
Average value: 62.5 MPa Grade Count:8
Elongation at Break 0.800 - 293 %0.800 - 293 %Average value: 34.1 % Grade Count:134
 2.50 - 70.0 %
@Temperature -40.0 - 150 °C
2.50 - 70.0 %
@Temperature -40.0 - 302 °F
Average value: 61.0 % Grade Count:9
Elongation at Yield 3.00 - 30.0 %3.00 - 30.0 %Average value: 10.4 % Grade Count:57
 3.00 - 42.0 %
@Temperature -40.0 - 120 °C
3.00 - 42.0 %
@Temperature -40.0 - 248 °F
Average value: 26.6 % Grade Count:8
Modulus of Elasticity 0.970 - 10.8 GPa141 - 1570 ksiAverage value: 2.93 GPa Grade Count:101
 0.320 - 4.09 GPa
@Temperature -40.0 - 150 °C
46.4 - 593 ksi
@Temperature -40.0 - 302 °F
Average value: 1.17 GPa Grade Count:8
Flexural Yield Strength 25.0 - 250 MPa3630 - 36300 psiAverage value: 90.0 MPa Grade Count:106
 17.0 - 183 MPa
@Temperature -40.0 - 120 °C
2470 - 26500 psi
@Temperature -40.0 - 248 °F
Average value: 86.2 MPa Grade Count:13
Flexural Modulus 0.600 - 9.20 GPa87.0 - 1330 ksiAverage value: 2.64 GPa Grade Count:111
 0.305 - 5.50 GPa
@Temperature -40.0 - 120 °C
44.2 - 798 ksi
@Temperature -40.0 - 248 °F
Average value: 1.39 GPa Grade Count:9
Compressive Yield Strength 27.0 - 95.0 MPa3920 - 13800 psiAverage value: 68.4 MPa Grade Count:6
Izod Impact, Notched 0.300 J/cm - NB0.562 ft-lb/in - NBAverage value: 0.979 J/cm Grade Count:52
 0.210 - 0.500 J/cm
@Temperature -40.0 - -30.0 °C
0.393 - 0.937 ft-lb/in
@Temperature -40.0 - -22.0 °F
Average value: 0.375 J/cm Grade Count:12
Izod Impact, Unnotched 10.7 - 5340 J/cm20.0 - 10000 ft-lb/inAverage value: 10.7 J/cm Grade Count:4
Izod Impact, Notched (ISO) 1.50 - 10.0 kJ/m²0.714 - 4.76 ft-lb/in²Average value: 5.17 kJ/m² Grade Count:25
 2.00 - 10.0 kJ/m²
@Temperature -40.0 - -30.0 °C
0.952 - 4.76 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 4.76 kJ/m² Grade Count:9
Izod Impact, Unnotched (ISO) 3.40 - 21000 kJ/m²1.62 - 9990 ft-lb/in²Average value: 41.9 kJ/m² Grade Count:10
Charpy Impact Unnotched 0.250 J/cm² - NB1.19 ft-lb/in² - NBAverage value: 6.35 J/cm² Grade Count:75
 4.10 - 2099.79 J/cm²
@Temperature -40.0 - -20.0 °C
19.5 - 9993.41 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 9.45 J/cm² Grade Count:27
Charpy Impact, Notched 0.100 - 10.1 J/cm²0.476 - 48.0 ft-lb/in²Average value: 0.913 J/cm² Grade Count:82
 0.200 - 1.60 J/cm²
@Temperature -40.0 - -20.0 °C
0.952 - 7.61 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.426 J/cm² Grade Count:36
Taber Abrasion, mg/1000 Cycles 5.00 - 6.005.00 - 6.00Average value: 5.17 Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+8 - 1.00e+18 ohm-cm1.00e+8 - 1.00e+18 ohm-cmAverage value: 1.20e+16 ohm-cm Grade Count:85
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 8.99e+13 ohm Grade Count:55
Dielectric Constant 3.00 - 8.003.00 - 8.00Average value: 4.50 Grade Count:38
Dielectric Strength 10.0 - 100 kV/mm254 - 2540 kV/inAverage value: 25.3 kV/mm Grade Count:66
Dissipation Factor 0.00300 - 0.1250.00300 - 0.125Average value: 0.0439 Grade Count:25
Arc Resistance 60.0 - 125 sec60.0 - 125 secAverage value: 113 sec Grade Count:7
Comparative Tracking Index 250 - 600 V250 - 600 VAverage value: 565 V Grade Count:71
Hot Wire Ignition, HWI 7.00 - 120 sec7.00 - 120 secAverage value: 46.3 sec Grade Count:7
High Amp Arc Ignition, HAI 120 arcs120 arcsAverage value: 120 arcs Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 100 µm/m-°C3.89 - 55.6 µin/in-°FAverage value: 71.9 µm/m-°C Grade Count:42
 75.0 - 75.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
41.7 - 41.7 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 75.0 µm/m-°C Grade Count:2
 75.0 - 75.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
41.7 - 41.7 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 75.0 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 59.4 - 140 µm/m-°C33.0 - 77.8 µin/in-°FAverage value: 89.1 µm/m-°C Grade Count:12
Specific Heat Capacity 3.73 J/g-°C0.891 BTU/lb-°FAverage value: 3.73 J/g-°C Grade Count:4
Thermal Conductivity 0.230 - 0.264 W/m-K1.60 - 1.83 BTU-in/hr-ft²-°FAverage value: 0.257 W/m-K Grade Count:5
Melting Point 198 - 225 °C388 - 437 °FAverage value: 220 °C Grade Count:89
Maximum Service Temperature, Air 70.0 - 185 °C158 - 365 °FAverage value: 116 °C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 135 - 215 °C275 - 419 °FAverage value: 182 °C Grade Count:71
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 210 °C122 - 410 °FAverage value: 74.3 °C Grade Count:116
Vicat Softening Point 160 - 240 °C320 - 464 °FAverage value: 201 °C Grade Count:41
Minimum Service Temperature, Air -60.0 - -40.0 °C-76.0 - -40.0 °FAverage value: -55.0 °C Grade Count:4
UL RTI, Electrical 65.0 - 130 °C149 - 266 °FAverage value: 108 °C Grade Count:9
UL RTI, Mechanical with Impact 65.0 - 105 °C149 - 221 °FAverage value: 73.8 °C Grade Count:9
UL RTI, Mechanical without Impact 65.0 - 125 °C149 - 257 °FAverage value: 89.5 °C Grade Count:9
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:122
Oxygen Index 25.0 - 37.0 %25.0 - 37.0 %Average value: 31.3 % Grade Count:19
Glow Wire Test 700 - 960 °C1290 - 1760 °FAverage value: 894 °C Grade Count:59
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 270 °C428 - 518 °FAverage value: 241 °C Grade Count:14
Nozzle Temperature 210 - 266 °C410 - 510 °FAverage value: 243 °C Grade Count:13
Melt Temperature 200 - 300 °C392 - 572 °FAverage value: 249 °C Grade Count:78
Mold Temperature 30.0 - 120 °C86.0 - 248 °FAverage value: 70.4 °C Grade Count:78
Drying Temperature 75.0 - 130 °C167 - 266 °FAverage value: 84.1 °C Grade Count:66
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.172 % Grade Count:36
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:3
Injection Pressure 4.96 - 130 MPa720 - 18900 psiAverage value: 77.0 MPa Grade Count:28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, Heat Stabilized
Overview of materials for Nylon 6, Impact Grade
Overview of materials for Nylon 6, Extruded
Overview of materials for Nylon 6, Cast

O2403 / 77964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.