MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: High moisture vapor transmission. Good physical properties and elasticity.

Uses: Blown and flat die/cast film extrusion.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Water Vapor Transmission  500 g/m²/day
@Temperature 23.0 °C
32.2 g/100 in²/day
@Temperature 73.4 °F
50% RH; ASTM E96B
 3000 g/m²/day
@Temperature 38.0 °C
193 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM D6701
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inflex bar, Injection
 0.0090 cm/cm0.0090 in/indisk, Injection
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 87 - 93
@Time 5.00 sec
87 - 93
@Time 0.00139 hour
ASTM D2240
Tensile Strength 34.5 MPa5000 psiASTM D412
Elongation at Break 550 %550 %ASTM D412
100% Modulus 6.20 MPa
@Strain 100 %
899 psi
@Strain 100 %
ASTM D412
300% Modulus 13.8 MPa
@Strain 300 %
2000 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.370 GPa53.7 ksiASTM D790
Tear Strength 78.9 kN/m450 pliTrouser; ASTM D470
Graves Tear Strength 21.0 kN/m120 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4040H18, 1000g; ASTM D3389
Compression Set  42 %
@Temperature 23.0 °C,
Time 79200 sec
42 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 61 %
@Temperature 70.0 °C,
Time 79200 sec
61 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Tensile Set 18 %18 %ASTM D412/D638
 18 %18 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 144 °C291 °FDSC
 155 °C311 °FKofler
Glass Transition Temp, Tg -24.0 °C-11.2 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 177 °C351 °FExtrusion
Zone 2 182 °C360 °FExtrusion
Zone 3 188 °C370 °FExtrusion
Zone 4 193 °C379 °FExtrusion
Adapter Temperature 199 °C390 °F5, Extrusion
Die Temperature 199 °C390 °FZone 1, Extrusion
 199 °C390 °FZone 2, Extrusion
Drying Temperature 82.0 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Volume Swell in Water40%24h @ 23°C, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin

PNOVEON039 / 55305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.