MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: High moisture vapor transmission. Good low temperature properties and elasticity.

Uses: Blown and flat die/cast film extrusion.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Vapor Transmission 650 g/m²/day41.9 g/100 in²/day23°C, 50% RH; ASTM D96B
 6500 g/m²/day
@Temperature 38.0 °C
419 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM D6701
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 77 - 83
@Time 5.00 sec
77 - 83
@Time 0.00139 hour
ASTM D2240
Tensile Strength 31.0 MPa4500 psiASTM D412
Elongation at Break 700 %700 %ASTM D412
100% Modulus 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
ASTM D412
300% Modulus 8.30 MPa
@Strain 300 %
1200 psi
@Strain 300 %
ASTM D412
Tear Strength 17.5 kN/m100 pliASTM D470
Graves Tear Strength 61.4 kN/m350 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 6060H18, 1000g; ASTM D3389
Tensile Set 10 %10 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °FDSC
 135 °C275 °FKofler
Glass Transition Temp, Tg -37.0 °C-34.6 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 171 °C340 °FExtrusion
Zone 2 177 °C351 °FExtrusion
Zone 3 182 °C360 °FExtrusion
Zone 4 188 °C370 °FExtrusion
Adapter Temperature 193 °C379 °FExtrusion
Die Temperature 193 °C379 °FZone 1, Extrusion
 193 °C379 °FZone 2, Extrusion
Drying Temperature 82.0 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58197 Ester Based Thermoplastic Polyurethane

PNOVEON042 / 55309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.