MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.

Uses: Blown and flat die/cast film extrusion, Injection and blow molding.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 89 - 95
@Time 5.00 sec
89 - 95
@Time 0.00139 hour
ASTM D2240
Tensile Strength 62.1 MPa9010 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
100% Modulus 9.00 MPa
@Strain 100 %
1310 psi
@Strain 100 %
ASTM D412
300% Modulus 22.9 MPa
@Strain 300 %
3320 psi
@Strain 300 %
ASTM D412
Tear Strength 29.8 kN/m170 pliASTM D470
Graves Tear Strength 105 kN/m600 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4040H18, 1000g; ASTM D3389 B
Tensile Set 16 %16 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 °C284 °FDSC
 170 °C338 °FKofler
Glass Transition Temp, Tg -45.0 °C-49.0 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 2.3 %2.3 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Zone 1 177 °C351 °FExtrusion
Zone 2 182 °C360 °FExtrusion
Zone 3 188 °C370 °FExtrusion
Zone 4 193 °C379 °FExtrusion
Adapter Temperature 199 °C390 °FExtrusion
Die Temperature 199 °C390 °FZone 1, Extrusion
 199 °C390 °FZone 2, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Volume swell in Water0.5%24h, 23°C; ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane

PNOVEON036 / 55302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.