MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.16 - 1.82 g/cc0.0419 - 0.0658 lb/in³Average value: 1.44 g/cc Grade Count:178
Filler Content 10.0 - 60.0 %10.0 - 60.0 %Average value: 25.3 % Grade Count:33
Water Absorption 0.600 - 8.00 %0.600 - 8.00 %Average value: 2.79 % Grade Count:45
Moisture Absorption at Equilibrium 0.170 - 4.00 %0.170 - 4.00 %Average value: 1.66 % Grade Count:44
Water Absorption at Saturation 3.50 - 9.00 %3.50 - 9.00 %Average value: 6.11 % Grade Count:22
Additive Loading 20.0 - 50.0 %20.0 - 50.0 %Average value: 32.2 % Grade Count:6
Maximum Moisture Content  0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000800 - 0.0150 cm/cm0.000800 - 0.0150 in/inAverage value: 0.00450 cm/cm Grade Count:141
Linear Mold Shrinkage, Transverse 0.00100 - 0.0158 cm/cm0.00100 - 0.0158 in/inAverage value: 0.00800 cm/cm Grade Count:83
Melt Flow 1.00 - 40.0 g/10 min1.00 - 40.0 g/10 minAverage value: 12.6 g/10 min Grade Count:40
Ash 15.0 - 30.0 %15.0 - 30.0 %Average value: 22.9 % Grade Count:7
 38.0 - 42.0 %
@Temperature 625 - 625 °C
38.0 - 42.0 %
@Temperature 1160 - 1160 °F
Average value: 40.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110 - 121110 - 121Average value: 119 Grade Count:18
Hardness, Shore D 80.0 - 90.080.0 - 90.0Average value: 87.2 Grade Count:5
Ball Indentation Hardness 70.3 - 370 MPa10200 - 53700 psiAverage value: 199 MPa Grade Count:18
Tensile Strength, Ultimate 30.0 - 220 MPa4350 - 31900 psiAverage value: 114 MPa Grade Count:168
 10.0 - 105 MPa
@Temperature 60.0 - 150 °C
1450 - 15200 psi
@Temperature 140 - 302 °F
Average value: 50.2 MPa Grade Count:6
Tensile Strength, Yield 50.0 - 210 MPa7250 - 30500 psiAverage value: 105 MPa Grade Count:19
Elongation at Break 1.00 - 50.0 %1.00 - 50.0 %Average value: 4.11 % Grade Count:170
 1.20 - 15.0 %
@Temperature 60.0 - 150 °C
1.20 - 15.0 %
@Temperature 140 - 302 °F
Average value: 6.45 % Grade Count:6
Elongation at Yield 2.00 - 14.0 %2.00 - 14.0 %Average value: 4.90 % Grade Count:15
 1.70 - 4.50 %
@Temperature 90.0 - 150 °C
1.70 - 4.50 %
@Temperature 194 - 302 °F
Average value: 2.95 % Grade Count:2
Modulus of Elasticity 1.00 - 18.6 GPa145 - 2700 ksiAverage value: 7.95 GPa Grade Count:131
 1.70 - 7.80 GPa
@Temperature 60.0 - 150 °C
247 - 1130 ksi
@Temperature 140 - 302 °F
Average value: 4.22 GPa Grade Count:6
Flexural Yield Strength 52.0 - 340 MPa7540 - 49300 psiAverage value: 172 MPa Grade Count:120
Flexural Modulus 2.30 - 17.9 GPa334 - 2600 ksiAverage value: 7.26 GPa Grade Count:126
Flexural Strain at Break 1.50 - 6.90 %1.50 - 6.90 %Average value: 3.51 % Grade Count:10
Izod Impact, Notched 0.280 - 1.80 J/cm0.525 - 3.37 ft-lb/inAverage value: 0.915 J/cm Grade Count:54
Izod Impact, Unnotched 4.81 - 10.7 J/cm9.00 - 20.0 ft-lb/inAverage value: 7.93 J/cm Grade Count:14
Izod Impact, Notched (ISO) 2.50 - 107 kJ/m²1.19 - 50.9 ft-lb/in²Average value: 10.1 kJ/m² Grade Count:44
 3.70 - 37.0 kJ/m²
@Temperature -40.0 - -30.0 °C
1.76 - 17.6 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 8.03 kJ/m² Grade Count:22
Izod Impact, Unnotched (ISO) 10.0 - 80.0 kJ/m²4.76 - 38.1 ft-lb/in²Average value: 43.5 kJ/m² Grade Count:23
 35.0 - 67.0 kJ/m²
@Temperature -30.0 - -30.0 °C
16.7 - 31.9 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 53.4 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.50 - 2100 J/cm²7.14 - 9990 ft-lb/in²Average value: 5.21 J/cm² Grade Count:99
 0.700 - 10.0 J/cm²
@Temperature -40.0 - -20.0 °C
3.33 - 47.6 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 4.43 J/cm² Grade Count:46
Charpy Impact, Notched 0.100 - 5.50 J/cm²0.476 - 26.2 ft-lb/in²Average value: 0.894 J/cm² Grade Count:104
 0.100 - 1.20 J/cm²
@Temperature -40.0 - -20.0 °C
0.476 - 5.71 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.609 J/cm² Grade Count:45
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm1.00e+11 - 1.00e+17 ohm-cmAverage value: 4.53e+15 ohm-cm Grade Count:69
Surface Resistance 1.00e+8 - 8.00e+15 ohm1.00e+8 - 8.00e+15 ohmAverage value: 5.77e+14 ohm Grade Count:51
Dielectric Constant 2.90 - 10.02.90 - 10.0Average value: 4.60 Grade Count:25
Dielectric Strength 9.00 - 70.0 kV/mm229 - 1780 kV/inAverage value: 28.7 kV/mm Grade Count:58
Dissipation Factor 0.00600 - 0.3000.00600 - 0.300Average value: 0.0729 Grade Count:21
Comparative Tracking Index 200 - 600 V200 - 600 VAverage value: 481 V Grade Count:83
Hot Wire Ignition, HWI 7.00 - 120 sec7.00 - 120 secAverage value: 103 sec Grade Count:6
High Amp Arc Ignition, HAI 15.0 - 120 arcs15.0 - 120 arcsAverage value: 114 arcs Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 82.0 µm/m-°C11.0 - 45.6 µin/in-°FAverage value: 41.9 µm/m-°C Grade Count:19
CTE, linear, Transverse to Flow 23.0 - 110 µm/m-°C12.8 - 61.1 µin/in-°FAverage value: 68.3 µm/m-°C Grade Count:9
Melting Point 216 - 260 °C420 - 500 °FAverage value: 222 °C Grade Count:96
Maximum Service Temperature, Air 80.0 - 200 °C176 - 392 °FAverage value: 133 °C Grade Count:20
Hot Ball Pressure Test 165 - 175 °C329 - 347 °FAverage value: 170 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 165 - 245 °C329 - 473 °FAverage value: 210 °C Grade Count:68
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 230 °C158 - 446 °FAverage value: 187 °C Grade Count:134
Vicat Softening Point 195 - 250 °C383 - 482 °FAverage value: 209 °C Grade Count:59
Minimum Service Temperature, Air -60.0 °C-76.0 °FAverage value: -60.0 °C Grade Count:9
UL RTI, Electrical 65.0 - 140 °C149 - 284 °FAverage value: 110 °C Grade Count:11
UL RTI, Mechanical with Impact 65.0 - 125 °C149 - 257 °FAverage value: 101 °C Grade Count:11
UL RTI, Mechanical without Impact 65.0 - 140 °C149 - 284 °FAverage value: 109 °C Grade Count:11
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:157
Oxygen Index 22.0 - 68.0 %22.0 - 68.0 %Average value: 30.8 % Grade Count:26
Glow Wire Test 600 - 960 °C1110 - 1760 °FAverage value: 898 °C Grade Count:99
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 300 °C428 - 572 °FAverage value: 257 °C Grade Count:23
Nozzle Temperature 210 - 280 °C410 - 536 °FAverage value: 248 °C Grade Count:14
Melt Temperature 210 - 300 °C410 - 572 °FAverage value: 254 °C Grade Count:114
Mold Temperature 30.0 - 120 °C86.0 - 248 °FAverage value: 76.5 °C Grade Count:118
Drying Temperature 75.0 - 130 °C167 - 266 °FAverage value: 85.3 °C Grade Count:110
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.167 % Grade Count:79
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:12
Injection Pressure 3.45 - 138 MPa500 - 20000 psiAverage value: 88.0 MPa Grade Count:50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled

O2420 / 77980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.