MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.16 - 1.82 g/ccAverage value: 1.44 g/cc Grade Count:178
Filler Content 10.0 - 60.0 %Average value: 25.3 % Grade Count:33
Water Absorption 0.600 - 8.00 %Average value: 2.79 % Grade Count:45
Moisture Absorption at Equilibrium 0.170 - 4.00 %Average value: 1.66 % Grade Count:44
Water Absorption at Saturation 3.50 - 9.00 %Average value: 6.11 % Grade Count:22
Additive Loading 20.0 - 50.0 %Average value: 32.2 % Grade Count:6
Maximum Moisture Content 0.200 - 0.200
@Temperature 120 - 120 °C
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000800 - 0.0150 cm/cmAverage value: 0.00450 cm/cm Grade Count:141
Linear Mold Shrinkage, Transverse 0.00100 - 0.0158 cm/cmAverage value: 0.00800 cm/cm Grade Count:83
Melt Flow 1.00 - 40.0 g/10 minAverage value: 12.6 g/10 min Grade Count:40
Ash 15.0 - 30.0 %Average value: 22.9 % Grade Count:7
 38.0 - 42.0 %
@Temperature 625 - 625 °C
Average value: 40.0 % Grade Count:1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110 - 121Average value: 119 Grade Count:18
Hardness, Shore D 80.0 - 90.0Average value: 87.2 Grade Count:5
Ball Indentation Hardness 70.3 - 370 MPaAverage value: 199 MPa Grade Count:18
Tensile Strength, Ultimate 30.0 - 220 MPaAverage value: 114 MPa Grade Count:168
 10.0 - 105 MPa
@Temperature 60.0 - 150 °C
Average value: 50.2 MPa Grade Count:6
Tensile Strength, Yield 50.0 - 210 MPaAverage value: 105 MPa Grade Count:19
Elongation at Break 1.00 - 50.0 %Average value: 4.11 % Grade Count:170
 1.20 - 15.0 %
@Temperature 60.0 - 150 °C
Average value: 6.45 % Grade Count:6
Elongation at Yield 2.00 - 14.0 %Average value: 4.90 % Grade Count:15
 1.70 - 4.50 %
@Temperature 90.0 - 150 °C
Average value: 2.95 % Grade Count:2
Modulus of Elasticity 1.00 - 18.6 GPaAverage value: 7.95 GPa Grade Count:131
 1.70 - 7.80 GPa
@Temperature 60.0 - 150 °C
Average value: 4.22 GPa Grade Count:6
Flexural Yield Strength 52.0 - 340 MPaAverage value: 172 MPa Grade Count:120
Flexural Modulus 2.30 - 17.9 GPaAverage value: 7.26 GPa Grade Count:126
Flexural Strain at Break 1.50 - 6.90 %Average value: 3.51 % Grade Count:10
Izod Impact, Notched 0.280 - 1.80 J/cmAverage value: 0.915 J/cm Grade Count:54
Izod Impact, Unnotched 4.81 - 10.7 J/cmAverage value: 7.93 J/cm Grade Count:14
Izod Impact, Notched (ISO) 2.50 - 107 kJ/m²Average value: 10.1 kJ/m² Grade Count:44
 3.70 - 37.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 8.03 kJ/m² Grade Count:22
Izod Impact, Unnotched (ISO) 10.0 - 80.0 kJ/m²Average value: 43.5 kJ/m² Grade Count:23
 35.0 - 67.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 53.4 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.50 - 2100 J/cm²Average value: 5.21 J/cm² Grade Count:99
 0.700 - 10.0 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 4.43 J/cm² Grade Count:46
Charpy Impact, Notched 0.100 - 5.50 J/cm²Average value: 0.894 J/cm² Grade Count:104
 0.100 - 1.20 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.609 J/cm² Grade Count:45
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cmAverage value: 4.53e+15 ohm-cm Grade Count:69
Surface Resistance 1.00e+8 - 8.00e+15 ohmAverage value: 5.77e+14 ohm Grade Count:51
Dielectric Constant 2.90 - 10.0Average value: 4.60 Grade Count:25
Dielectric Strength 9.00 - 70.0 kV/mmAverage value: 28.7 kV/mm Grade Count:58
Dissipation Factor 0.00600 - 0.300Average value: 0.0729 Grade Count:21
Comparative Tracking Index 200 - 600 VAverage value: 481 V Grade Count:83
Hot Wire Ignition, HWI 7.00 - 120 secAverage value: 103 sec Grade Count:6
High Amp Arc Ignition, HAI 15.0 - 120 arcsAverage value: 114 arcs Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.8 - 82.0 µm/m-°CAverage value: 41.9 µm/m-°C Grade Count:19
CTE, linear, Transverse to Flow 23.0 - 110 µm/m-°CAverage value: 68.3 µm/m-°C Grade Count:9
Melting Point 216 - 260 °CAverage value: 222 °C Grade Count:96
Maximum Service Temperature, Air 80.0 - 200 °CAverage value: 133 °C Grade Count:20
Hot Ball Pressure Test 165 - 175 °CAverage value: 170 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 165 - 245 °CAverage value: 210 °C Grade Count:68
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 230 °CAverage value: 187 °C Grade Count:134
Vicat Softening Point 195 - 250 °CAverage value: 209 °C Grade Count:59
Minimum Service Temperature, Air -60.0 °CAverage value: -60.0 °C Grade Count:9
UL RTI, Electrical 65.0 - 140 °CAverage value: 110 °C Grade Count:11
UL RTI, Mechanical with Impact 65.0 - 125 °CAverage value: 101 °C Grade Count:11
UL RTI, Mechanical without Impact 65.0 - 140 °CAverage value: 109 °C Grade Count:11
Flammability, UL94 HB - 5VAGrade Count:157
Oxygen Index 22.0 - 68.0 %Average value: 30.8 % Grade Count:26
Glow Wire Test 600 - 960 °CAverage value: 898 °C Grade Count:99
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 300 °CAverage value: 257 °C Grade Count:23
Nozzle Temperature 210 - 280 °CAverage value: 248 °C Grade Count:14
Melt Temperature 210 - 300 °CAverage value: 254 °C Grade Count:114
Mold Temperature 30.0 - 120 °CAverage value: 76.5 °C Grade Count:118
Drying Temperature 75.0 - 130 °CAverage value: 85.3 °C Grade Count:110
Moisture Content 0.0300 - 0.200 %Average value: 0.167 % Grade Count:79
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:12
Injection Pressure 3.45 - 138 MPaAverage value: 88.0 MPa Grade Count:50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Overview of materials for Nylon 6, 20% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled

O2420 / 77980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.