MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) CAF® 4 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 4 is a one component silicone elastomer which cures at room temperature
  • Acetic
  • Self-leveling
  • Off-white
Applications: CAF 4 is mainly used in industrial sealing, bonding and coating applications: It is notably used for:
  • bonding of plastics in aeronautics,
  • electrical insulation,
  • coating of fabrics for thermal protection,
  • coating of conveyor belts.
Advantages: CAF 4 is quick curing, has very good mechanical properties, good heat stability and high dielectric properties. CAF 4 therefore provides perfect assembly and complete sealing between different materials subject to thermal stresses.

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, ISO R 1183
  • Specific Gravity, ASTM D297, after curing
  • Brookfield Viscosity, ASTM D445
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Shear Strength, on aluminum AG3, curing 7d at 23°C
  • Tear Strength, ASTM D624
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D419
  • Dissipation Factor, ASTM D150
  • Thermal Conductivity, Standard NF x 10021
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air, Peak
  • Minimum Service Temperature, Air
  • Brittleness Temperature
  • Cure Time, Skin Formation Time
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.