MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) CAF® 4 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 4 is a one component silicone elastomer which cures at room temperature
  • Acetic
  • Self-leveling
  • Off-white
Applications: CAF 4 is mainly used in industrial sealing, bonding and coating applications: It is notably used for:
  • bonding of plastics in aeronautics,
  • electrical insulation,
  • coating of fabrics for thermal protection,
  • coating of conveyor belts.
Advantages: CAF 4 is quick curing, has very good mechanical properties, good heat stability and high dielectric properties. CAF 4 therefore provides perfect assembly and complete sealing between different materials subject to thermal stresses.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccISO R 1183
 1.19 g/ccafter curing; ASTM D297
Brookfield Viscosity 250000 cPASTM D445
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37ASTM D2240
Tensile Strength 551 psiASTM D412
Elongation at Break 290 %ASTM D412
100% Modulus 0.116 ksi
@Strain 100 %
ASTM D412
Shear Strength 1.20 MPa
@Thickness 1.00 mm
on aluminum AG3, curing 7d at 23°C
Tear Strength 25.7 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 533 V/milASTM D419
Dissipation Factor 0.0021
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.300 W/m-K
@Temperature 30.0 °C
Standard NF x 10021
Maximum Service Temperature, Air 225 °C
@Thickness 2.00 mm,
Time 3.60e+6 sec
 250 °C
@Thickness 2.00 mm,
Time 259000 sec
Peak
Minimum Service Temperature, Air -60.0 °C
@Thickness 2.00 mm,
Time 3.60e+6 sec
Brittleness Temperature -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 minSkin Formation Time
 5.00 hour
@Thickness 2.00 mm
 
Descriptive Properties
Appearanceviscous flowing paste
ColorOff-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) CAF® 730 Silicone Rubber
Overview of materials for Acrylic, Cast
Overview of materials for Silicone Rubber
Overview of materials for Acrylic, General Purpose, Molded
Elkem (Bluestar Silicones) CAF® 7037 Silicone Rubber

PBLUST088 / 191064

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.