Description: CAF 7037 is a one-component silicone elastomer that cures at room temperature:- OXIME
- FLUID
- BRICK RED
- HIGH RELEASE CAPACITY
It is particularly suited to coating, protection and assembly applications.Applications: - Continuous coating of conveyor belts.
- Insulating of electrical motors.
- Sealing of iron bases.
- Sealing of air filters.
- Silk screening of gaskets.
Advantages: - Low viscosity for coating applications.
- Non-corrosive.
- Long pot life.
- Good temperature resistance (250°C peak).
- Good dielectric properties.
Information provided by Bluestar Silicones |