MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ArcelorMittal MartINsite® 1500 Cold Rolled Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: The family of MartINsite® steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming method such as roll forming. To achieve maximum weight reduction while maintaining a very good anti-intrusion during the crash properties, some parts require the use of UHSS, such as the sills and door reinforcements, have simple shapes, and therefore the steel is slightly deformed. For this reason, ArcelorMittal has complemented its offer with the family of MartINsite® steels with very high yield strength delivery and interesting properties of bending deformation and a very good formability of the cut edges.

Application: Thanks to their excellent mechanical properties, these grades are particularly suitable for automotive safety parts for shock resistance. Typical parts are shown in the figure below:

  • Front and rear bumper beams
  • Door beam
  • Side Sill Reinforcement
  • Roof cross member

Information provided by ArcelorMittal

Vendors:
Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, L0=80 mm, th<3 mm
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Carbon, C
  • Iron, Fe, as balance
  • Manganese, Mn
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.