MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ArcelorMittal MartINsite® 1500 Cold Rolled Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: The family of MartINsite® steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming method such as roll forming. To achieve maximum weight reduction while maintaining a very good anti-intrusion during the crash properties, some parts require the use of UHSS, such as the sills and door reinforcements, have simple shapes, and therefore the steel is slightly deformed. For this reason, ArcelorMittal has complemented its offer with the family of MartINsite® steels with very high yield strength delivery and interesting properties of bending deformation and a very good formability of the cut edges.

Application: Thanks to their excellent mechanical properties, these grades are particularly suitable for automotive safety parts for shock resistance. Typical parts are shown in the figure below:

  • Front and rear bumper beams
  • Door beam
  • Side Sill Reinforcement
  • Roof cross member

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1200 - 1700 MPa
Tensile Strength, Yield 1200 - 1500 MPa
Elongation at Break >= 3.0 %L0=80 mm, th<3 mm
Fatigue Strength <= 880 MPa
@# of Cycles 2.00e+6
 <= 880 MPa
@# of Cycles 1.00e+7
 <= 930 MPa
@# of Cycles 100000
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.25 %
Iron, Fe >= 97.25 %as balance
Manganese, Mn <= 2.0 %
Silicon, Si <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
Carpenter AerMet® 310
ArcelorMittal Dual Phase 600 Very High Strength Cold Rolled Steel
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled
AISI Type A10 Tool Steel

NARCE006 / 159914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.