| SSAB Docol 600FB is a modern hot-rolled advanced high strength steel with a matrix of ferrite or strengthened ferrite containing bainite or strengthened bainite and with a refined grain size. The steel grade is well suited for cold formed automotive components such as wheels, chassis components and different structural reinforcements. Formability is very good, especially in hole expansion. SSAB Docol HR440Y580T-FB meets the requirements of HR440Y580T-FB according to VDA 239-100. Dimension Range: Hot rolled / UC: thickness 2.00-4.00 mm, width up to 1600 mm. Hot rolled / GI: thickness 2.00-5.00 mm, width up to 1450 mm. Slit strip and cut to length sheets are available upon request. Data provided by SSAB. |