MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with conventional airless equipment. Spark testable, non-shrinking 100% solids. ARC HT-S is reinforced with high modulus reinforcements to improve long term resistance to cold wall induced blistering and delamination. Its unique chemistry allows for reliable long term immersion service at elevated temperatures without the need for post curing thereby simplifying installation. ARC HT-S is capable of in-situ curing.

Benefits:

  • High voltage spark testable to NACE SP 0188
  • Capable of ambient cure
  • Two color system provides visual indicators of mixing
  • Able to handle immersion in elevated temperature aqueous applications

Suggested Uses:

  • Process Cooling Water Heat Exchangers
  • Crystallizers/Evaporators
  • Centrifuges
  • Condensate Return Pumps
  • Distillation Units
  • Oil/Water, Oil/Gas Separator Vessels

Information provided by Chesterton

Vendors:
Available Properties
  • Density, Cured
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D790
  • Adhesive Bond Strength, ASTM D4541
  • Maximum Service Temperature, Air, Wet Service
  • Maximum Service Temperature, Air, Dry Service
  • Cure Time, Overcoat Begin
  • Cure Time, Overcoat Begin
  • Cure Time, Overcoat Begin
  • Cure Time, Overcoat Begin
  • Cure Time, Overcoat End
  • Cure Time, Overcoat End
  • Cure Time, Overcoat End
  • Cure Time, Overcoat End
  • Cure Time, Full Mechanical
  • Cure Time, Full Chemical
  • Cure Time, Full Mechanical
  • Cure Time, Full Chemical
  • Cure Time, Full Mechanical
  • Cure Time, Full Chemical
  • Cure Time, Full Mechanical
  • Cure Time, Full Chemical
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.