MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Aptek 2100-A7C/B Low modulus urethane staking compound
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although APTEK 2100-A7C/B is capable of achieving full cure at room temperature, a short term exposure to moderate heat will greatly reduce processing time and optimize cured properties.

100% solids, solvent free system that will not form voids during cure or service life; Low Tg for excellent low-temperature cycling and performance; Very good substrate adhesion, superior to silicones; Exceeds NASA outgassing requirements for high vacuum environments

APTEK 2100-A7C is a translucent, filled polyol resin. APTEK 2100-B is a yellow/orange, organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors:
Available Properties
  • Density, A Component; ASTM D1475
  • Density, B Component; ASTM D1475
  • Viscosity, B Component; ASTM D1824
  • Outgassing - Total Mass Loss, Cured property; at 10E-6 torr; ASTM E-595
  • Collected Volatile Condensable Material, Cured property; at 10E-6 torr; ASTM E595
  • Hardness, Shore A, Cured property; ASTM D2240
  • Tensile Strength, Ultimate, Cured property; ASTM D412
  • Elongation at Break, Cured property; ASTM D412
  • Volume Resistivity, Cured property; ASTM D257
  • Dielectric Constant, ASTM D150, Cured property
  • Dielectric Strength, Cured property; 0.1 inch; ASTM D149
  • Dissipation Factor, ASTM D150, Cured property
  • CTE, linear, JMTP P200, Cured property; alpha 1
  • CTE, linear, JMTP P200, Cured property; alpha 2
  • Glass Transition Temp, Tg, Cured property; JMTP 200
  • Flash Point, A Component; ASTM D92
  • Flash Point, B Component; ASTM D92
  • Processing Temperature, Cure 5 hrs + 2 hrs at RT
  • Processing Temperature, Cure 3 hrs + 2 hrs at RT
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.