MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Sika SikaBond® T55 Trowel Grade Polyurethane Elastic Adhesive for Wood Flooring
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: SikaBond-T55 is a one-component, low-VOC, permanently elastic, crack bridging, super strong polyurethane adhesive for full surface bonding of wood flooring.

Where to Use SikaBond-T55 may be used for solid and engineered wood floors (strips, longstrips, planks, panels, boards) mosaic parquet, industrial parquet, wood paving (residential) as well as chip boards can be bonded.

Advantages:

  • 400% Elongation
  • Formulated to be extremely easy to trowel, preventing arm strain
  • Fast curing - unfinished wood flooring can be sanded after 12 hours of cure time
  • Crack bridging
  • Suitable for most common types of wood floors
  • Especially good for problematic woods such as beech and bamboo
  • Suitable for bonding wood floors directly onto old ceramic tiles
  • Suitable for in-floor radiant heat installation
  • Footfall-sound-dampening adhesive
  • Contains no water
  • Bonds solid wood flooring up to 8 inches wide and engineered planks up to 14 inches wide directly to concrete with no length limitations
  • Eliminate sleepers and plywood over concrete and gypsum substrates
  • Permanently elastic – allows planks to expand and contract without damage to the adhesive or substrate

Information provided by Sika Corporation.

Vendors:
Available Properties
  • Density
  • Hardness, Shore A, after 28 days
  • Tensile Strength
  • Elongation at Break, 50% RH
  • Shear Strength, 1 mm adhesive thickness at 73°F (23°C) and 50% RH
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, 50% RH, Skinning/Laying time
  • Cure Time, Floor may accept light foot traffic
  • Cure Time, sanded
  • Cure Time, 50% RH
  • Shelf Life, in original unopened cartridge
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.