MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sika SikaBond® T55 Trowel Grade Polyurethane Elastic Adhesive for Wood Flooring
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: SikaBond-T55 is a one-component, low-VOC, permanently elastic, crack bridging, super strong polyurethane adhesive for full surface bonding of wood flooring.

Where to Use SikaBond-T55 may be used for solid and engineered wood floors (strips, longstrips, planks, panels, boards) mosaic parquet, industrial parquet, wood paving (residential) as well as chip boards can be bonded.

Advantages:

  • 400% Elongation
  • Formulated to be extremely easy to trowel, preventing arm strain
  • Fast curing - unfinished wood flooring can be sanded after 12 hours of cure time
  • Crack bridging
  • Suitable for most common types of wood floors
  • Especially good for problematic woods such as beech and bamboo
  • Suitable for bonding wood floors directly onto old ceramic tiles
  • Suitable for in-floor radiant heat installation
  • Footfall-sound-dampening adhesive
  • Contains no water
  • Bonds solid wood flooring up to 8 inches wide and engineered planks up to 14 inches wide directly to concrete with no length limitations
  • Eliminate sleepers and plywood over concrete and gypsum substrates
  • Permanently elastic – allows planks to expand and contract without damage to the adhesive or substrate

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35after 28 days
Tensile Strength 217 psi
Elongation at Break 400 %50% RH
Shear Strength 145 psi1 mm adhesive thickness at 73°F (23°C) and 50% RH
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 158 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hourFloor may accept light foot traffic
 12.0 hoursanded
 45.0 - 60.0 min50% RH, Skinning/Laying time
 24.0 hour
@Thickness 4.00 mm,
Temperature 23.0 °C
50% RH
Shelf Life 12.0 Month
@Temperature 10.0 - 25.0 °C
in original unopened cartridge
 
Descriptive Properties
Chemical Base1-component polyurethanemoisture curing
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA922 / 209829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.