MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
ChevronTexaco ISO 32 Machine Oil R&O LVI
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Machine Oil R&O LVI is a superior quality naphthenic lubricating oil

It is formulated with highly refined base stock with rust inhibiting, antioxidant, and foam suppressant additives.

Applications

Chevron Machine Oil R&O LVI is formulated to give outstanding service in a wide variety of applications

The low pour properties of Chevron Machine Oil R&O LVI make it excellent for service in telemotor systems, hydraulic door checks, hydraulic jacks, railway signal mechanisms, and similar equipment operating intermittently, particularly in low ambient temperatures.

Chevron Machine Oil R&O LVI is recommended for:

  • air compressor cylinder lubrication, particularly when deposit formation is a problem due to higher than normal discharge air temperatures and/or oil feed rates are higher than generally recommended.
  • reciprocating air compressor cranckcases, in order to consolidate lubricant requirements
  • circulating oil systems of large compressors used in the manufacture of ammonia. Chevron Machine Oil R&O LVI will not react with the ammonia to form deleterious deposits in the system
  • low temperature applications, particularly in the power generation field, for use in gas turbine complexes
Do not use in high pressure systems in the vicinity of flames, sparks, and hot surfaces. Use only in well ventilated areas. Keep container closed.

Key Words: CPS Number: 230320; MSDS Number: 7668
Vendors:
Available Properties
  • API Gravity
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Oxidative Stability, ASTM D943, Hours to 2.0 mg KOH/g acid number
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.