MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Assab Steels ASSAB XW-41 Cold Work Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Chrome-moly Steel; Tool Steel; Cold Work Steel

Material Notes: XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:
  • High wear resistance
  • High compressive strength
  • Good through-hardening properties
  • High stability in hardening
  • Good resistance to tempering-back.

XW-41 is used when cutting thicker, harder materials; when forming with tools subjected to bending stresses and where high impact loads are involved. XW-41 can be supplied in various finishes, including the hot-rolled, pre-machined and fine machined condition. It is also available in the form of hollow bar and rings.

AISI D2, W.-Nr. 1.2379

Vendors:
Available Properties
  • Density
  • Density
  • Density
  • Hardness, Rockwell C, 1020°C Austenitizing temperature, for tempering at 650°C
  • Hardness, Rockwell C, 1050°C Austenitizing temperature, for tempering at 650°C
  • Hardness, Rockwell C, 1020°C Austenitizing temperature, for tempering at 550°C
  • Hardness, Rockwell C, 1050°C Austenitizing temperature, for tempering at 400°C
  • Hardness, Rockwell C, 1020°C Austenitizing temperature, for tempering at 400°C
  • Hardness, Rockwell C, 1050°C Austenitizing temperature, for tempering at 200°C
  • Hardness, Rockwell C, At 980°C during hardening, soaking time 30 minutes
  • Hardness, Rockwell C, 1050°C Austenitizing temperature, for tempering at 550°C
  • Hardness, Rockwell C, Hardened and tempered.
  • Hardness, Rockwell C, At 980°C during hardening, soaking time 60 minutes
  • Hardness, Rockwell C, 1020°C Austenitizing temperature, for tempering at 200°C
  • Hardness, Rockwell C, At 1060°C during hardening, soaking time 30 minutes
  • Hardness, Rockwell C, At 1020°C during hardening, soaking time 30 minutes
  • Hardness, Rockwell C, At 1020°C during hardening, soaking time 60 minutes
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Compressive Strength, HRC 55 Rc0.2
  • Compressive Strength, HRC 62 Rc0.2.
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.