MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Braskem TN2006 EVA General Film Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. Additionally, this product has a good water vapor barrier. The melt properties allow processability in tubular film equipment, being able to be coextruded in combination with many others materials. It contains antioxidant additives. Its applications include: heat seal layer in coextruded and laminated films, food packaging, hood stretch films, base polymer for agricultural films, and geomembranes.

Vendors:
Available Properties
  • Density, ASTM-D1505
  • Vinyl Acetate Content
  • Melt Flow, ASTM-D1238
  • Hardness, Shore A, ASTM-D2240
  • Hardness, Shore D, ASTM-D2240
  • Tensile Strength at Break, ASTM-D638
  • Film Elongation at Break, MD, ASTM-D882
  • Film Elongation at Break, TD, ASTM-D882
  • Elongation at Break, ASTM-D638
  • Secant Modulus, MD, ASTM-D882, 2% Secant Modulus
  • Secant Modulus, TD, ASTM-D882, 2% Secant Modulus
  • Elmendorf Tear Strength MD, ASTM-D1922
  • Elmendorf Tear Strength TD, ASTM-D1922
  • Elmendorf Tear Strength, MD, ASTM-D1922
  • Elmendorf Tear Strength, TD, ASTM-D1922
  • Dart Drop, ASTM-D1709 (Method B)
  • Dart Drop Test, ASTM-D1709 (Method B)
  • Film Tensile Strength at Break, MD, ASTM-D882
  • Film Tensile Strength at Break, TD, ASTM-D882
  • Melting Point, ASTM-D3418
  • Vicat Softening Point, ASTM-D1525
  • Haze, ASTM-D1003
  • Gloss, ASTM-D2457, Angle 45°
  • Die Opening, Blow Film Extrusion
  • Blow-up Ratio (BUR), Blow Film Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.