MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Braskem TN2006 EVA General Film Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. Additionally, this product has a good water vapor barrier. The melt properties allow processability in tubular film equipment, being able to be coextruded in combination with many others materials. It contains antioxidant additives. Its applications include: heat seal layer in coextruded and laminated films, food packaging, hood stretch films, base polymer for agricultural films, and geomembranes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM-D1505
Vinyl Acetate Content 18 %
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89ASTM-D2240
Hardness, Shore D 39ASTM-D2240
Tensile Strength at Break 33.0 MPaASTM-D638
Film Elongation at Break, MD 450 %ASTM-D882
Film Elongation at Break, TD 700 %ASTM-D882
Elongation at Break 680 %ASTM-D638
Secant Modulus, MD 0.0390 GPa2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.0380 GPa2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 145 gASTM-D1922
Elmendorf Tear Strength TD 345 gASTM-D1922
Elmendorf Tear Strength, MD 2.90 g/micronASTM-D1922
Elmendorf Tear Strength, TD 6.90 g/micronASTM-D1922
Dart Drop 12.0 g/micronASTM-D1709 (Method B)
Dart Drop Test 600 gASTM-D1709 (Method B)
Film Tensile Strength at Break, MD 32.0 MPaASTM-D882
Film Tensile Strength at Break, TD 31.0 MPaASTM-D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 90.0 °CASTM-D3418
Vicat Softening Point 70.0 °C
@Load 1.02 kg
ASTM-D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %ASTM-D1003
Gloss 87 %Angle 45°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Die Opening 0.100 - 0.150 cmBlow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0Blow Film Extrusion
 
Descriptive Properties
Mass Temperature (°C)175-190Blow Film Extrusion
Temperature Profile (°C)150-190Blow Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade
Braskem CN8092 EVA Molding Copolymer
Braskem TN2005 EVA General Film Copolymer
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer

PBRAS816 / 106662

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.