MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a, allowing for use in packing or holding food during cooking when used unmodified and according to good manufacturing practices for food contact application.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Key Words: ULDPE, VLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.912 g/cc0.0329 lb/in³
Moisture Vapor Transmission 0.0300 cc-mm/m²-24hr-atm0.0762 cc-mil/100 in²-24hr-atmor 1.2 g/m²/atm/24 hr
Thickness 25.0 microns0.984 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg
1.0 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.2.
 
Mechanical PropertiesMetricEnglishComments
Elmendorf Tear Strength MD 385 g385 g
Elmendorf Tear Strength TD 499 g499 g
Elmendorf Tear Strength, MD 15.4 g/micron391 g/mil
Elmendorf Tear Strength, TD 20.0 g/micron508 g/mil
Dart Drop >= 33.2 g/micron>= 843 g/mil
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 95.0 °C203 °F
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %6.0 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 96.0 °C205 °FSeal initiation temperature
 226 °C439 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade
ExxonMobil Exceed™ 3512CB Film Resin
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin

PDW413 / 34482

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.