MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP51 Fast Curing High Bond Strength Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Suitable for bonding and sealing
  • Easy handling
  • Fast setting
  • Very rapid curing
  • Cryogenically serviceable
Product Description: Master Bond EP51 is a high performing “5 minute” type system featuring rapid curing and convenient handling. What differentiates Master Bond’s iteration of this kind of product is that it is offered as a standard product and also in customized versions with variations in viscosity and color being readily available. EP51 has a forgiving one to one mix ratio by weight or volume. It is important to clarify a common misconception on “5 minute” epoxies. In reality, the working life is in the 5 minute range; the actual fixturing or set up time can range from 10-20 minutes depending the application and ambient temperature. Full curing also depends on these parameters and can range from 12-18 hours. Upon polymerization, the system has a high tensile lap shear strength along with good chemical resistance. Most importantly, EP51 has been successfully used in a number of cryogenic applications over the broad temperature range of 4K to +250°F. It bonds well to a wide array of substrates, including composites, metals, glass, ceramics and many rubbers and plastics. EP51 offers typically superior epoxy type electrically insulative properties. It can be used in aerospace, specialty OEM and related applications, particularly for repair. It is also useful in situations where a faster curing system for prototyping is desirable.

Product Advantages:

  • Non-critical one to one mix ratio by weight or volume
  • Easy application, adhesive spreads evenly and smoothly
  • Fast cure at ambient temperatures
  • High bonding strength to a wide variety of substrates
  • Available in various viscosities and colors
  • Serviceable at cryogenic temperatures down to 4K

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.