MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570°F (300°C). Used for semiconductor lead frames in integrated circuits, bi-metal thermostat strip, thermostat rods, for ceramic-to-metal seals with alumina ceramics, and various glass-to-metal seals such as the core of copper-clad wire for sealing into glass envelopes of electric bulbs, radio valves, television tubes, and fluorescent lights. Standard product forms are tube, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS K94100; ASTM F 30, B 753; DIN 17745; S.E.W. 385; Werkstoff Nr. 1.3917; AFNOR NF A54-301
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, Annealed prior to test
  • Tensile Strength, Ultimate, Annealed prior to test
  • Tensile Strength, Yield, Annealed prior to test
  • Tensile Strength, Yield, Annealed prior to test
  • Elongation at Break, Annealed prior to test.
  • Elongation at Break, Annealed prior to test.
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Nickel, Ni, nominal; adjustable to meet expansion requirements
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Special Metals (includes the former Inco Alloys International Inc.)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.