MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570°F (300°C). Used for semiconductor lead frames in integrated circuits, bi-metal thermostat strip, thermostat rods, for ceramic-to-metal seals with alumina ceramics, and various glass-to-metal seals such as the core of copper-clad wire for sealing into glass envelopes of electric bulbs, radio valves, television tubes, and fluorescent lights. Standard product forms are tube, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS K94100; ASTM F 30, B 753; DIN 17745; S.E.W. 385; Werkstoff Nr. 1.3917; AFNOR NF A54-301
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.11 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 490 MPaAnnealed prior to test
 430 MPa
@Temperature 300 °C
Annealed prior to test
Tensile Strength, Yield 250 MPa
@Strain 0.2 %
Annealed prior to test
 120 MPa
@Strain 0.2 %,
Temperature 300 °C
Annealed prior to test
Elongation at Break 42 %Annealed prior to test.
 42 %
@Temperature 300 °C
Annealed prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.30 µm/m-°C
@Temperature 20.0 - 100 °C
 4.50 - 6.50 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 10.5 W/m-K
Melting Point 1435 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.15 %
Carbon, C <= 0.050 %
Chromium, Cr <= 0.25 %
Cobalt, Co <= 1.0 %
Iron, Fe 55 %As remainder
Manganese, Mn <= 0.80 %
Nickel, Ni 42 %nominal; adjustable to meet expansion requirements
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.30 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
California Fine Wire Alloy 52 Nickel Iron Alloy
FloMet Fe-42% Ni Controlled Expansion Alloy
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)

NIND21 / 17525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.