MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Dow HPL 502 Carboxylated Terpolymer Latex  (discontinued **)
Categories: Polymer

Material Notes: Applications: HPL*502 Latex is part of Dow’s HPL* Latex family of the high-performance ignition resistant latexes. HPL* latexes offer properties not available in standard styrene-butadiene latexes. HPL* latex products have chlorine content reacted into the backbone of the polymer that provides a “built in” level of ignition resistance. This inherent ignition resistance enables the formulator to displace some or all of the alumina trihydrate (ATH) with less costly calcium carbonate filler which may result in substantial compound cost savings. The presence of chlorine in the polymer backbone also allows the use of an antimony synergist without the addition of expensive additives. HPL* latexes are used in the precoat compound for both commercial and residential carpet backing applications. HPL* latexes are also used in unitary and tile backing applications.

Benefits:

  • High Solids
  • Ignition Resistant
  • Blister Resistant
  • Medium Hand

Vendors:
Available Properties
  • Density
  • Solids Content
  • Particle Size
  • pH
  • Brookfield Viscosity, #2 @ 50 rpm
  • Glass Transition Temp, Tg
  • Oxygen Index, 0 ATH Load
  • Oxygen Index, 200 ATH Load
  • Oxygen Index, 400 ATH Load
  • Oxygen Index, 600 ATH Load
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.