MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow HPL 502 Carboxylated Terpolymer Latex  (discontinued **)
Categories: Polymer

Material Notes: Applications: HPL*502 Latex is part of Dow’s HPL* Latex family of the high-performance ignition resistant latexes. HPL* latexes offer properties not available in standard styrene-butadiene latexes. HPL* latex products have chlorine content reacted into the backbone of the polymer that provides a “built in” level of ignition resistance. This inherent ignition resistance enables the formulator to displace some or all of the alumina trihydrate (ATH) with less costly calcium carbonate filler which may result in substantial compound cost savings. The presence of chlorine in the polymer backbone also allows the use of an antimony synergist without the addition of expensive additives. HPL* latexes are used in the precoat compound for both commercial and residential carpet backing applications. HPL* latexes are also used in unitary and tile backing applications.

Benefits:

  • High Solids
  • Ignition Resistant
  • Blister Resistant
  • Medium Hand

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Solids Content 57 %
Particle Size 1.25 µm
pH 7.0
Brookfield Viscosity 300 cP#2 @ 50 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 9.50 °C
Oxygen Index 26 %0 ATH Load
 30 %200 ATH Load
 36 %400 ATH Load
 40 %600 ATH Load
 
Descriptive Properties
Minimum film formation temperature48.2°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg P650 Epichlorohydrin
Honeywell HPL 6001 Lubricant Blend
Overview of materials for Chlorosulfonated Polyethylene Rubber
ATG s.r.l. CO-ECO Epichlorohydrin Rubber
Overview of materials for Melamine-Phenolic Copolymer

PDWST095 / 142304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.