MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
ChevronTexaco ISO 320 Paper Machine Oil D
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Paper Machine Oils D are manufactured using select high viscosity index, paraffinic base stocks. Their additive packages include rust, oxidation, and foam inhibitors as well as an effective detergent for deposit control. The oxidation products that result from high temperature operation, as well as dirt, water, and particle fines are effectively dispersed by the detergent. In addition, these oils impart mild EP characteristics to minimize wear and have excellent water separating ability (demulsibility). These oils also have excellent wet filterability with fine porosity oil filters, as demonstrated by the Pall Filterability Test.

Applications

The Chevron Paper Machine Oil D series is recommended for use in paper machine circulating systems, dryer bearings, and calender stacks. Chevron Paper Machine Oils D have had extensive field service lubricating Valmet, Beloit, and Voith Sulzer paper machine equipment.

Chevron Paper Machine Oils D ISO 150, 220, and 320 may be used as AGMA R&O Oils 4, 5, and 6, respectively, for enclosed gear drives. Chevron Paper Machine Oils D ISO 220 and 320 may also be used in plain and antifriction bearings at elevated ambient temperatures as high as 80°C (175°F).

Key Words: CPS Number: 253022; MSDS Number: 6694
Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Oxidative Stability
  • Timken Test
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.