| The high-strength structural steel at 1100 MPa Strenx 1100MC is a hot-rolled structural steel made for cold forming, with a minimum yield strength of 1100 MPa for stronger and lighter structures. These cut-to-length sheets feature excellent thickness accuracy and surface quality in relation to strength level, providing an outstanding finish to the final products. Typical applications include a wide range of parts and components such as demanding load-bearing structures. Dimension Range: Strenx 1100MC is available as cut to length sheets with mill edge in thicknesses of 3.00 - 8.00 mm, widths up to 1700 mm and lengths up to 16 meters. Data provided by SSAB. |