MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Ampco Metal AMPCO® 22 Aluminum Bronze, Extruded Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: AMPCO 22 is a duplex structure alloy of approx. 50 % of each phase - gamma 2 and beta. It has good hardness, excellent compression and wear resistance and sliding properties. As the elongation of the material is very low, thin sections should be avoided and the material should be well backed up.

Applications: The field of service of AMPCO 22, with few exceptions, is limited to forming and/or drawing stainless steel, especially when runs are long or gauge is heavy and it is essential that tolerances be maintained.

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, HB 30
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Compressive Yield Strength, Proportional Limit
  • Compressive Yield Strength, 0.1% Perm. Set
  • Compressive Strength
  • Izod Impact
  • Charpy Impact
  • Electrical Resistivity, 10% I.A.C.S.
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Aluminum, Al
  • Copper, Cu, As Balance
  • Iron, Fe
  • Other, total
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.