MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® 22 Aluminum Bronze, Extruded Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: AMPCO 22 is a duplex structure alloy of approx. 50 % of each phase - gamma 2 and beta. It has good hardness, excellent compression and wear resistance and sliding properties. As the elongation of the material is very low, thin sections should be avoided and the material should be well backed up.

Applications: The field of service of AMPCO 22, with few exceptions, is limited to forming and/or drawing stainless steel, especially when runs are long or gauge is heavy and it is essential that tolerances be maintained.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.06 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 332HB 30
Hardness, Rockwell C 35
Tensile Strength, Ultimate 724 MPa
Tensile Strength, Yield 427 MPa
@Strain 0.2 %
Elongation at Break 0.50 %
Reduction of Area 0.00 %
Modulus of Elasticity 103 GPa
Compressive Yield Strength 241 MPaProportional Limit
 510 MPa0.1% Perm. Set
Compressive Strength 1351 MPa
Izod Impact 2.70 J
Charpy Impact 2.70 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000167 ohm-cm10% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 42.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 14.4 %
Copper, Cu 78.4 - 80.9 %As Balance
Iron, Fe 4.7 %
Other, total <= 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCO® 21 Aluminum Bronze, Round, ≤ 50.8 mm.
MetalTek MTEK 275 Cast UNS C95900 Aluminum Bronze
Beryllium Copper, UNS C17300, TM08 Temper Strip
Ampco Metal AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
Ampco Metal AMPCO® 21 Aluminum Bronze, Rectangular

NAMPCO18 / 14972

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.