MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfaces and is very thixotropic to resist running and sagging. This product gives very good vibration and impact resistance. It gives good resistance to water, salt spray, inorganic acids and bases and most organic solvents. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. EP11HTFS Gray will reach initial cure at room temperature within 2 – 4 hours with full cure in 24 – 48 hours. Cure time can be accelerated by the application of heat. Times and temperatures from 1 hour at 65°C to 15 minutes at 100°C are typical for most applications. Time to heat substrate must be taken into account. Cooler temperatures will also extend work time and increase cure times.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors:
Available Properties
  • Specific Gravity, TM R050-16, Part A
  • Specific Gravity, TM R050-16, Mixed
  • Specific Gravity, TM R050-16, Part B
  • Water Absorption, TM R050-35
  • Viscosity, TM R050-12, Part B, RVT, #7, 2.5 rpm
  • Viscosity, TM R050-12, Mixed
  • Viscosity, TM R050-12, Part A, RVT, #7, 2.5 rpm
  • Hardness, Shore D, TM R050-17
  • Tensile Strength at Break, TM R050-36
  • Tensile Strength, Ultimate, TM R050-36
  • Tensile Strength, Yield, TM R050-36
  • Elongation at Break, TM R050-36
  • Tensile Modulus, TM R050-36
  • Compressive Yield Strength, TM R050-38
  • Compressive Strength, TM R050-38, Break
  • Compressive Strength, TM R050-38, Ultimate
  • Compressive Modulus, TM R050-38
  • Adhesive Bond Strength, TM R050-37, Lap shear; 2024 T3 Al Abraded / MEK Wipe
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, TM R050-25
  • Cure Time
  • Cure Time
  • Pot Life, TM R050-19, Mass: 50g
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.