Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfaces and is very thixotropic to resist running and sagging. This product gives very good vibration and impact resistance. It gives good resistance to water, salt spray, inorganic acids and bases and most organic solvents. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. EP11HTFS Gray will reach initial cure at room temperature within 2 – 4 hours with full cure in 24 – 48 hours. Cure time can be accelerated by the application of heat. Times and temperatures from 1 hour at 65°C to 15 minutes at 100°C are typical for most applications. Time to heat substrate must be taken into account. Cooler temperatures will also extend work time and increase cure times.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company. |