MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Unifrax Fiberfrax® Duraset® Flet
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers in a product form with lower densities and increased mat thickness. Felt products are compressible but resilient; they conform to irregular surfaces yet have sufficient integrity to hold their shape in gaskets and formed parts. Both felt grades are wet laid, uniform, ceramic fiber mats which have been impregnated with a thermosetting resin. In Lo-Con flet, this resin has been precured to produce a semi-flexible rolled sheet. The binders in Duraset have been left uncured so they can be molded under heat and pressure to retain a complex shape after processing. The organic binders remain functional at low and moderate temperatures (to 650°F); however, the core ceramic fiber materials will provide consistent performance at temperatures well in excess of 2000°F, providing excellent thermal insulation in a wide range of applications.

Fiberfax Duraset is a lightweight mat made from spun Fiberfrax ceramic fibers which have been impregnated with a thermosetting resin. Supplied in uncured form, it can be formed with the simultaneous application of pressure and heat to achieve complex shapes of rigid consistency for thermal and acoustical shielding. Use of Fiberfrax spun fibers allows for production of parts with severe draws without tearing during the forming process. Duraset flet is an excellent insulator with a high temperature use limit. If wet by water or steam, thermal and physical properties remain unaffected after drying. Duraset felt is unaffected by most chemicals except hydrofluoric and phosphoric acids and concentrated alkalies.

    Product Advantages
  • Formability
  • Flexibility
  • High temperature stability
  • Low thermal conductivity
  • Low heat storage
  • Weight reduction
  • Thermal shock resistance
  • High heat reflectance
  • Excellent corrosion resistance
  • Easy to wrap, shape, and cut

    Typical Applications
  • Automotive Exhaust Heat Shield
  • Commercial Fire Protection Applications
  • Aerospace Heat Shielding

Information Provided by Unifrax I LLC

Vendors:
Available Properties
  • Specific Gravity
  • Density, Nominal Core Density
  • Loss On Ignition
  • Melting Point
  • Maximum Service Temperature, Air, Recommended Operating Temperature
  • Cure Time
  • Al2O3
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Unifrax I LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.