MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Duraset® Flet
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers in a product form with lower densities and increased mat thickness. Felt products are compressible but resilient; they conform to irregular surfaces yet have sufficient integrity to hold their shape in gaskets and formed parts. Both felt grades are wet laid, uniform, ceramic fiber mats which have been impregnated with a thermosetting resin. In Lo-Con flet, this resin has been precured to produce a semi-flexible rolled sheet. The binders in Duraset have been left uncured so they can be molded under heat and pressure to retain a complex shape after processing. The organic binders remain functional at low and moderate temperatures (to 650°F); however, the core ceramic fiber materials will provide consistent performance at temperatures well in excess of 2000°F, providing excellent thermal insulation in a wide range of applications.

Fiberfax Duraset is a lightweight mat made from spun Fiberfrax ceramic fibers which have been impregnated with a thermosetting resin. Supplied in uncured form, it can be formed with the simultaneous application of pressure and heat to achieve complex shapes of rigid consistency for thermal and acoustical shielding. Use of Fiberfrax spun fibers allows for production of parts with severe draws without tearing during the forming process. Duraset flet is an excellent insulator with a high temperature use limit. If wet by water or steam, thermal and physical properties remain unaffected after drying. Duraset felt is unaffected by most chemicals except hydrofluoric and phosphoric acids and concentrated alkalies.

    Product Advantages
  • Formability
  • Flexibility
  • High temperature stability
  • Low thermal conductivity
  • Low heat storage
  • Weight reduction
  • Thermal shock resistance
  • High heat reflectance
  • Excellent corrosion resistance
  • Easy to wrap, shape, and cut

    Typical Applications
  • Automotive Exhaust Heat Shield
  • Commercial Fire Protection Applications
  • Aerospace Heat Shielding

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.73 g/cc
Density 9.50 lb/ft³Nominal Core Density
Loss On Ignition 9.0 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1260 °CRecommended Operating Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 - 2.00 min
@Temperature 204 - 232 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 40 - 45 %
SiO2 50 - 55 %
 
Descriptive Properties
ColorYellow/Tan
Fiber Index (% Wt)70
Other Inorganics (%)<5
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Lo-Con™ Felt
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation

CUNIF055 / 97827

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.