MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Lo-Con™ Felt
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers in a product form with lower densities and increased mat thickness. Felt products are compressible but resilient; they conform to irregular surfaces yet have sufficient integrity to hold their shape in gaskets and formed parts. Both felt grades are wet laid, uniform, ceramic fiber mats which have been impregnated with a thermosetting resin. In Lo-Con flet, this resin has been precured to produce a semi-flexible rolled sheet. The binders in Duraset have been left uncured so they can be molded under heat and pressure to retain a complex shape after processing. The organic binders remain functional at low and moderate temperatures (to 650°F); however, the core ceramic fiber materials will provide consistent performance at temperatures well in excess of 2000°F, providing excellent thermal insulation in a wide range of applications.

Fiberfrax Lo-Con felt is a lightweight, flexible batting created from Fiberfrax Bulk ceramic fibers interlocked to form a strong, resilient insulation. It is manufactured by a unique wet felting process which removes unfiberized particles to produce a clean, efficient ceramic fiber felt insulation. A small amount of non-flaming organic binder is added to provide improved handling properties for easier installation in applications where organic burnout at low temperatures is acceptable.

    Product Advantages
  • Formability
  • Flexibility
  • High temperature stability
  • Low thermal conductivity
  • Low heat storage
  • Weight reduction
  • Thermal shock resistance
  • High heat reflectance
  • Excellent corrosion resistance
  • Easy to wrap, shape, and cut

    Typical Applications
  • Exhaust Duct Insulation
  • Commercial Appliances
  • Home Security Boxes
  • Expansion Joints
  • Domestic Appliances
  • Gasketing and Sealing

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.73 g/cc2.73 g/cc
Density 0.0737 g/cc0.00266 lb/in³Nominal Core Density
Loss On Ignition 4.0 %4.0 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1260 °C2300 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 40 - 45 %40 - 45 %
SiO2 50 - 55 %50 - 55 %
 
Descriptive Properties
ColorTan
Fiber Index (% Wt)70
Other Inorganics (%)<5
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Cerablanket AC2 Thermal Ceramic
DIAB Divinycell® F 50 Sandwich Core Material
Unifrax Insulfrax® S Blanket Insulation
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation
Overview of materials for Phenolic/Rubber; Molded

CUNIF054 / 97826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.