MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-704 Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-101 is an ultra low molecular weight fluoroelastomer. At room temperature it is an opaque paste. At temperatures above 70°C (158 °F) it becomes a transparent, viscous fluid. DAI-EL® G-101 is not crosslinkable but is used as a plasticizer in other fluoroelastomers.

Typical Applications: Additive for other DAI-EL® fluoroelastomers. Mechanical property data shows effect of G-101 plasticizer on DAI-EL® G-704 Fluoroelastomer.

Information provided by Daikin.

Vendors:
Available Properties
  • Specific Gravity, DAI-EL® G-101
  • Viscosity, DAI-EL® G-101
  • Molecular Weight, DAI-EL® G-101
  • Evaporation Loss, DAI-EL® G-101
  • Hardness, Shore A, G-704, 20 PHR G101 added
  • Hardness, Shore A, G-704, 0 PHR G101 added
  • Hardness, Shore A, After Air Aging, G-704, 20 PHR G101 added
  • Hardness, Shore A, After Air Aging, G-704, 0 PHR G101 added
  • Tensile Strength at Break, G-704, 20 PHR G101 added
  • Tensile Strength at Break, G-704, 0 PHR G101 added
  • Tensile Strength at Break, After Air Aging, G-704, 20 PHR G101 added
  • Tensile Strength at Break, After Air Aging, G-704, 0 PHR G101 added
  • Elongation at Break, G-704, 0 PHR G101 added
  • Elongation at Break, G-704, 20 PHR G101 added
  • Elongation at Break, After Air Aging, G-704, 0 PHR G101 added
  • Elongation at Break, After Air Aging, G-704, 20 PHR G101 added
  • 100% Modulus, G-704, 20 PHR G101 added
  • 100% Modulus, G-704, 0 PHR G101 added
  • Volume Resistivity, DAI-EL® G-101
  • Dissipation Factor, DAI-EL® G-101
  • Dissipation Factor, DAI-EL® G-101
  • Specific Heat Capacity, DAI-EL® G-101
  • Refractive Index, DAI-EL® G-101
  • Cure Time, Press cure, G-704
  • Cure Time, Oven cure, G-704
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.