MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications.

Advantages & Application Notes:

  • This product is a color-coded, black and opaque version of the industry standard EPO-TEK® 353ND-T epoxy adhesive.
  • Suggested applications:
    • Semiconductor, glob top DAM around IC’s, using COB or DCA packaging formats
    • Electronics Assembly
      • Insulating adhesive for bonding stainless steel metals, ceramics and carbon composites used in ink-jetting heads
      • Insulating and plugging wires and feed-through cables of automotive circuits
      • Hard Disk Drive – thixotropic staking and termination of Al and Cu coils
      • Adhesive for brushless motors and Cu coil windings
    • Medical
      • Light blocking in endoscopes, camera optics and IR sensor devices
    • Optical
  • Fiber optic component packaging: bonding fibers, active optics, metals, ceramics and plastic
Available in alternative viscosities and color

Information Provided by Epoxy Technology

Vendors:
Available Properties
  • Specific Gravity, Part B
  • Specific Gravity, Part A
  • Particle Size
  • Viscosity, 20 rpm
  • Hardness, Shore D
  • Tensile Modulus, Storage
  • Shear Strength, Lap
  • Shear Strength, Die
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Continuous
  • Minimum Service Temperature, Air, Intermittent
  • Glass Transition Temp, Tg, Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
  • Decomposition Temperature, Degradation Temperature
  • Transmission, Visible, Spectral
  • Transmission, Visible, Spectral
  • Cure Time, Minimum Bond Line
  • Cure Time, Minimum Bond Line
  • Cure Time, Minimum Bond Line
  • Cure Time, Minimum Bond Line
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.