MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Supreme 42HT-2 is a solvent-free, toughened, two part epoxy system featuring heat and chemical resistance. It has good thermal cycling capabilities and is ideal for bonding, sealing and encapsulating dissimilar substrates. Supreme 42HT-2 has a mix ratio of 100 to 40 by weight or 100 to 50 by volume. It adheres well to a wide variety of substrates including metals, many plastics, ceramics and glass. It is serviceable from -65°F to +425°F. The color of Part A is tan to brown and the color of Part B is amber. The cured epoxy has good electrical insulation properties. Most noteworthy, it will resist a wide variety of chemicals including many acids, bases, solvents, fuels and oils. It can be used in many industries including aerospace, electronic, chemical, OEM and many other fields. To optimize its product properties, the best cure schedule for Supreme 42HT-2 is overnight at room temperature followed by a few hours at 150-200°F. A paste, non-drip version called Supreme 42HT-2ND2 is also available. Additionally, this product will have only minimal flow if heat is added during curing.

Product Advantages:

  • Non-critical mix ratio: 100 to 40 by weight and 100 to 50 by volume
  • Easy application with conventional equipment
  • Solvent-free
  • Convenient cure schedules at both ambient and elevated temperatures
  • Excellent chemical resistance to acids, bases, fuels, oils and solvents
  • Good thermal stability up to +425°F
  • Longer working life
  • Good thermal cycling capabilities
Key Features
  • Toughened
  • Good thermal cycling capabilities
  • High temperature resistant
  • Chemical resistant

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Shear Strength, Tensile lap, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram mass
  • Shelf Life, in original unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.